3'-6"W x 5'H 3 Stage Stainless Steel Washer

Opening: 3'-6"W x 5'H

Line Speed: 4 FPM

Total Dimensions: 10'W x 12'H x 50'L

Manufacturer: Falcon Finishing

Stage 1: Clean. 90 Seconds@ 140 Degrees

Stage 2: Rinse. 60 Seconds @ Ambient

Stage 3: Rinse. 60 Seconds @ Ambient